Evaluation of Preheating Composite Resins for Repairing Resin Nanoceramic Restorations


Creative Commons License

ÖZCİVELEK T., Özcan B., Kasar B., Kılıçarslan M. A.

Meandros Medical And Dental Journal, cilt.26, sa.4, ss.436-445, 2025 (ESCI, TRDizin)

  • Yayın Türü: Makale / Tam Makale
  • Cilt numarası: 26 Sayı: 4
  • Basım Tarihi: 2025
  • Doi Numarası: 10.69601/meandrosmdj.1762141
  • Dergi Adı: Meandros Medical And Dental Journal
  • Derginin Tarandığı İndeksler: Emerging Sources Citation Index (ESCI), TR DİZİN (ULAKBİM)
  • Sayfa Sayıları: ss.436-445
  • Anahtar Kelimeler: CAD-CAM, Ceramics, Polymers, Composite resins, Nanocomposites, Dental restoration repair
  • Açık Arşiv Koleksiyonu: AVESİS Açık Erişim Koleksiyonu
  • Sağlık Bilimleri Üniversitesi Adresli: Evet

Özet

Objective: Resin nanoceramic dental restorations may need repair. This study evaluates the shear bond strength (SBS) of two composite resins applied at two temperatures to repair two resin nanoceramic materials. Materials and Methods: Ninety-six specimens were sliced from Lava Ultimate and CeraSmart resin nanoceramic blocks and subjected to thermal aging. Following surface roughness measurements, specimens were divided into eight subgroups(n=12) based on repair material and application temperature. Resin nanoceramic specimens were repaired using a Teflon mold with RubyCompP or RubyCompNano composite resins at 23°C or 50°C. All specimens were subjected to a SBS test at a 0.5mm/min crosshead speed until failure. Failure types were classified at 5X magnification. Statistical analysis of SBS test results was performed by a three-way ANOVA test, followed by post hoc Tukey’s pairwise comparisons(α=0.05). The relationship between failure modes and resin nanoceramic, composite resin, or preheating was analyzed with a chi-square test. Results: Surface roughness of resin nanoceramics was not statistically different(p>0.05). The resin nanoceramic type and preheating of repair materials had a significant effect on SBS(p=0.006, p<0.001). Results of three-way ANOVA displayed substantial differences among groups(p=0.038). Tukey’s pairwise comparisons revealed significant differences between SBS values for LavaUltimate repaired with posterior composite(LP) and CeraSmart repaired with preheated posterior composite(CPP) (p=0.034), LP and CeraSmart repaired with preheated nano composite(CNP) (p=0.030), CeraSmart repaired with nano composite(CN) and CPP(p=0.035), and CN-CNP(p=0.030). Mixed failure was predominant among groups. Conclusion: These findings imply that repairing CeraSmart resin nanoceramic and preheating the repair composite resin to 50°C attenuated the shear bond strength.